GA-2525
Herchy
| Berdestbûnî: | |
|---|---|
| Hejmar: | |
Test: Rêjeya A/B ya 1:1, 130°C x 5min x 15MPa
| Parametreyên hilberê | |||||||
| Mal | GA-2525 | GA-2530 | GA-2540 | GA-2850 | GA-2860 | GA-2870 | |
| Xuyabûnî | Translucent | ||||||
| Vîskozîtî (Pa.s) |
80 | 80 | 80 | 220 | 300 | 400 |
|
| Zehmetî (ShoreA) | 25 | 30 | 40 | 50 |
60 |
70 |
|
| Tûrbûn (g/cm3) | 1.08 | 1.10 | 1.11 | 1.13 | 1.14 |
1.16 |
|
| Hêza tîrêjê (MPa) | 4.5 |
5.0 |
5.5 |
6.0 |
6.0 |
5.0 |
|
| Dirêjbûn(%) | 400 | 350 | 300 | 250 | 220 |
180 |
|
| Hêza hêsirê (kN/m) | 12 | 14 | 18 |
20 | 18 |
16 |
|
| Linearshrinkage(%) | 2.0 | 2.0 | 2.0 | 2.0 | 2.0 |
2.0 |
|