GA-2525
Herchy
| Ku kumeka: | |
|---|---|
| Nhlayo: . | |
Xikambelo: Nhlayo ya A/B ya 1 :1, 130°C x 5min x 15MPa
| Tipharamitha ta swikumiwa | |||||||
| Ximakiwa | GA-2525 | GA-2530 | GA-2540 | GA-2850 | GA-2860 | GA-2870 | |
| Xivumbeko | Ku vonakala loku vonakaka | ||||||
| Ku tsindziyela(Pa.s) . |
80 | 80 | 80 | 220 | 300 | 400 |
|
| Ku nonoka (ShoreA) . | 25 | 30 | 40 | 50 |
60 |
70 |
|
| Ku tsindziyela(g/cm3) . | 1.08 | 1.10 | 1.11 | 1.13 | 1.14 |
1.16 |
|
| Ku tiya ka ku tsana (MPa) . | 4.5 |
5.0 |
5.5 |
6.0 |
6.0 |
5.0 |
|
| Ku leha(%) . | 400 | 350 | 300 | 250 | 220 |
180 |
|
| Matimba ya ku handzuka (kN/m) . | 12 | 14 | 18 |
20 | 18 |
16 |
|
| Ku hunguteka ka milayeni(%) . | 2.0 | 2.0 | 2.0 | 2.0 | 2.0 |
2.0 |
|