GA-2525 LSR fun Idi Gbogbogbo (Silica precipitated) (LSR)

Ohun elo: o dara fun iṣelọpọ awọn ipese idana, awọn ọja ile-iṣẹ oriṣiriṣi ati awọn ọja agba, bbl
Awọn ẹya ara ẹrọ: agbara giga, itọra ti o dara julọ.
  • GA-2525

  • Herchy

Wiwa:
Opoiye:

Idanwo: Ipin A/B ti 1: 1, 130°C x 5min x 15MPa


Ọja sile
Ọja GA-2525 GA-2530 GA-2540 GA-2850 GA-2860 GA-2870
Ifarahan Translucent

Igi (Pa.s)
80 80 80 220 300 400
Lile ( ShoreA) 25 30 40 50
60
70
Ìwúwo (g/cm3) 1.08 1.10 1.11 1.13 1.14
1.16
Agbara fifẹ (MPa) 4.5
5.0
5.5
6.0
6.0
5.0
Ilọsiwaju(%) 400 350 300 250 220
180
Agbara omije (kN/m) 12 14 18
20 18
16
Laini idinku(%) 2.0 2.0 2.0 2.0 2.0
2.0







Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ kiakia

Awọn ọja WA

IBI IWIFUNNI

Fi kun: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tẹli / WhatsApp / Skype: +86 15221953351
Aṣẹ-lori-ara     2023 Shanghai Herchy Rubber Co., Ltd. Maapu aaye |   Asiri Afihan | Atilẹyin Nipasẹ Leadong.