GA-2525 LSR ad Consilium generale (Silica praecipitatum) (LSR)

Applicatio: apta ad commeatus producendos, insedit andadult industrialis productis, etc.
Clavis lineamenta: robur excelsum, optimum fluidum.
  • GA-2525

  • Herchy

Availability:
Quantity:

Test: A/B proportio 1 :1, 130°C x 5min x 15MPa


Product parametri
Productum GA-2525 GA-2530 GA-2540 GA-2850 GA-2860 GA-2870
Aspectus Translucens

Viscositas (Pa.s)
80 80 80 220 300 400
Duritia (ShoreA) 25 30 40 50
60
70
Densitas (g/cm3) 1.08 1.10 1.11 1.13 1.14
1.16
Roboris distrahentes (MPa) 4.5
5.0
5.5
6.0
6.0
5.0
Prolongatio(%) 400 350 300 250 220
180
Robur scindere (kN/m) 12 14 18
20 18
16
Linearshrinkage(%) 2.0 2.0 2.0 2.0 2.0
2.0







Priora: 
Next: 

ORIGINAL LINKS

Our Products

Contact Information

Add: No.33, Lane CLIX, Taiye via, Fengxian District, Shanghai
Tel / whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Flexilis Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.