Momekano: Ratio A/B ya 1 :1, 130°C x 5min x 15MPa
| Ba paramètres ya produit | |||||||
| Eloko | GA-2525 na mokanda | GA-2530 oyo ezali na kati | GA-2540 oyo ezali na kati | GA-2850 na nzela ya mokanda | GA-2860 na mokanda | GA-2870 | |
| Komonana | Translucide ezali | ||||||
| Viscosité(Pa.s) ya . |
80 | 80 | 80 | 220 | 300 | 400 |
|
| Bokasi ya makasi (ShoreA) . | 25 | 30 | 40 | 50 |
60 |
70 |
|
| Densité(g/cm3) Ezali na ba . | 1.08 | 1.10 | 1.11 | 1.13 | 1.14 |
1.16 |
|
| Bokasi ya kokangama (MPa) . | 4.5 |
5.0 |
5.5 |
6.0 |
6.0 |
5.0 |
|
| Elongation(%) ya . | 400 | 350 | 300 | 250 | 220 |
180 |
|
| Bokasi ya kopasola (kN/m) . | 12 | 14 | 18 |
20 | 18 |
16 |
|
| Bokiti ya linéaire(%) . | 2.0 | 2.0 | 2.0 | 2.0 | 2.0 |