GA-2031W mphira wamadzimadzi wosagwira moto wa silikoni womangira (LSR)

Ntchito: Zoyenera kupanga zozimitsa moto pamagalimoto, zosindikizira kapena zokutira pazida zamagetsi, ndi zinthu zina zozimitsa moto. 
Zofunikira zazikulu: zomwe zimagwiritsidwa ntchito poponderezana ndi jekeseni, mitundu imatha kusintha, UL94V-0.
  • GA-2031W

  • Herchy

kupezeka:
kuchuluka:

Kuyesa: A/B chiŵerengero cha 1 :1, 130°C x 5min x 15MPa


Mankhwala magawo
Zogulitsa GA-2031W GA-2041W GA-2051W GA-2061W GA-2071W
(A/B) Mawonekedwe (Pamene/Wakuda) (Pamene/Wakuda) (Pamene/Wakuda) (Pamene/Wakuda) (Pamene/Wakuda)
Kuuma (ShoreA) 32
43
50
60
70
Kachulukidwe (g/cm3)

1.3

1.3 1.36 1.36 1.52
Mphamvu yamagetsi (MPa) 4.5
4.5
5.0
4.5
4.0
Kutalikira (%) 300 300 300 200 140
Mphamvu yamisozi (kN/m) 10 10 12
12 8.0









Zam'mbuyo: 
Ena: 

MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.