GA-2031W Pa'u silicone vai e taofia afi mo le fa'apipi'iina (LSR)

Talosaga: talafeagai mo le gaosia o taavale afi afi, faʻamaufaʻailoga poʻo ufiufi mo mea faʻaeletoroni, ma isi mea faʻagata afi. 
Vaega autu: faʻaaogaina mo le faʻamalosi ma tui tui, lanu e mafai ona fetuunai, UL94V-0.
  • GA-2031W

  • Herchy

Avanoa:
Aofaiga:

Su'ega: fua faatatau A/B ole 1:1, 130°C x 5min x 15MPa


Fa'atauga o oloa
Oloa GA-2031W GA-2041W GA-2051W GA-2061W GA-2071W
(A/B)Fa'aaliga (A'o/uliuli) (A'o/uliuli) (A'o/uliuli) (A'o/uliuli) (A'o/uliuli)
Malosi (ShoreA) 32
43
50
60
70
Malosi (g/cm3)

1.3

1.3 1.36 1.36 1.52
Malosi fa'amalosi (MPa) 4.5
4.5
5.0
4.5
4.0
Fa'atele(%) 300 300 300 200 140
Malosi o loimata (kN/m) 10 10 12
12 8.0









Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AALIGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.