Sinov: A/B nisbati 1:1, 130°C x 5min x 15MPa
| Mahsulot parametrlari | ||||||
| Mahsulot | GA-2031W | GA-2041W | GA-2051W | GA-2061W | GA-2071W | |
| (A/B) Tashqi ko'rinish | (Qora/Qora) | (Qora/Qora) | (Qora/Qora) | (Qora/Qora) | (Qora/Qora) | |
| Qattiqlik (ShoreA) | 32 |
43 |
50 |
60 |
70 |
|
| Zichlik (g/sm3) | 1.3 |
1.3 | 1.36 | 1.36 | 1.52 | |
| Kuchlanish kuchi (MPa) | 4.5 |
4.5 |
5.0 |
4.5 |
4.0 |
|
| Uzayish (%) | 300 | 300 | 300 | 200 | 140 |
|
| Yirilish kuchi (kN/m) | 10 | 10 | 12 |
12 | 8.0 |
|