Tel: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
Prodakt dɛn .
Yu de ya: Os » Prodakt dɛn . » Sintesis rɔba . » VMQ silikon na di . » GA-2031W Faya-retardant likwid silikon rɔba fɔ kɔmpreshɔn moldin (LSR)

Loading na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na .

Share to:
Fɛsbuk sherin bɔtin .
Twitter sherin bɔtin .
Layn sherin bɔtin .
WeChat sherin button .
LinkedIn Sharing bɔtin .
Pinterest Sharing bɔtin .
WhatsApp Sharing bɔtin .
ShareThis Sharing bɔtin .

GA-2031W faya-retardant likwid silikon rɔba fɔ kɔmpreshɔn moldin (LSR)

Aplikeshɔn: fayn fɔ prodyuz ɔtomotiv faya-retardant prodak, sil ɔ kɔva fɔ ilɛktronik aplayans, ɛn ɔda faya-ritardant difrɛn tin dɛn. 
Ki ficha: yuz fɔ kɔmpreshɔn ɛn injɛkshɔn mold, kɔlɔ dɛn na adjɔstabl,UL94V-0.
  • GA-2031W we de na di wɔl

  • Herchy na di .

Di tin dɛn we yu kin gɛt:
Kwantiti: .

Test: A/B ratio na 1 :1, 130°C x 5min x 15MPa


Prodakt Paramita dɛn .
Sɔntin GA-2031W we de na di wɔl GA-2041W we de na di wɔl GA-2051W we de na di wɔl GA-2061W we de na di wɔl GA-2071W we de na di wɔl
(A/B)Di we aw pɔsin de luk (While/Blak) (While/Blak) (While/Blak) (While/Blak) (While/Blak)
Hadnɛs (Shorea) . 32
43
50
60
70
Densiti(g/cm3) .

1.3

1.3 1.36 1.36 1.52
Tensil Strɔng (MPA) . 4.5
4.5
5.0
4.5
4.0
Elongeshɔn(%) . 300 300 300 200 140
Strɔng fɔ wata (KN/M) . 10 10 12
12 8.0









Bifo: 
Nɛks: 

Kwik Links .

Wi Prodakt dɛn .

Kɔntakt infɔmeshɔn .

Add: No.33, Lane 159, Taiye Rod, Fengxian Distrikt, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kopirayt     2023 Shanghai Herchy Rubber Co., Ltd. Saytmap . |   Prayvesi Polisi | Sɔpɔt bay . Leadong.