GA-99X1
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175心5minx 15MPa.
| Product parameters | |||||
| Product | GA-9931 | GA-9941 | GA-9951 | GA-9961 | GA-9971 |
| Appearance | Translucent | ||||
| Williamplasticity | 120 | 130 | 150 | 170 | 180 |
| Hardness (ShoreA) | 30 | 40 | 50 | 60 | 70 |
| Density(g/cm3) | 1.1 | 1.11 | 1.12 | 1.14 | 1.16 |
| Tensile strength (MPa) | 6 | 6 | 6 | 6 | 6.5 |
| Elongation(%) | 800 | 500 | 250 | 200 | 150 |
| Tear strength (kN/m) | 15 | 15 | 15 | 15 | 15 |
| 175"C x22h Compression Set(%) | 15 | 10 | 8 | 8 | 10 |