GA-91X0
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x5minx15MPa
| Product parameters | |||||
| Product | GA-9130 | GA-9140 | GA-9150 | GA-9160 | GA-9170 |
| Appearance | Translucent | ||||
| Williamplasticity | 150 | 190 | 250 | 280 | 300 |
| Hardness (ShoreA) | 30 | 40 | 50 | 60 | 70 |
| Density(g/cm3) | 1.11 | 1.14 | 1.17 | 1.20 | 1.21 |
| Tensile strength (MPa) | 8.0 | 9.5 | 10.0 | 9.0 | 8.5 |
| Elongation(%) | 900 | 700 | 600 | 500 | 400 |
| Tear strength (kN/m) | 17 | 20 | 25 | 25 | 25 |
| Surface resistance(Ω) | 1011 | ||||