GA-99X1
Herchy
| kupezeka: | |
|---|---|
| kuchuluka: | |
Kuyesa: 1% yochiritsa (50% phala la DBPMH mu chingamu cha silicone), 175心5minx 15MPa.
| Zogulitsa katundu | |||||
| Zogulitsa | GA-9931 | GA-9941 | GA-9951 | GA-9961 | GA-9971 |
| Maonekedwe | Zowoneka bwino | ||||
| Williamplasticity | 120 | 130 | 150 | 170 | 180 |
| Kuuma (ShoreA) | 30 | 40 | 50 | 60 | 70 |
| Kachulukidwe (g/cm3) | 1.1 | 1.11 | 1.12 | 1.14 | 1.16 |
| Mphamvu yamagetsi (MPa) | 6 | 6 | 6 | 6 | 6.5 |
| Kutalikira (%) | 800 | 500 | 250 | 200 | 150 |
| Mphamvu yamisozi (kN/m) | 15 | 15 | 15 | 15 | 15 |
| 175'C x22h Compression Set(%) | 15 | 10 | 8 | 8 | 10 |