GA-99X1 Ṣeto Ipaba Kekere Ṣeto rọba Silikoni (HCR)

Ohun elo: o dara fun iṣelọpọ oruka lilẹ, awọn ibusun, awọn ẹya adaṣe ati awọn ọja miiran.
Ẹya bọtini: resilience giga, ṣeto funmorawon kekere, HSE ti ko ni itọwo majele, ijẹrisi ti RoHS, REACH ati FDA.
  • GA-99X1

  • Herchy

Wiwa:
Opoiye:

Idanwo: 1% ti oluranlowo imularada (50% lẹẹ DBPMH ni silikoni gomu), 175心5minx 15MPa.


Ọja sile
Ọja GA-9931 GA-9941 GA-9951 GA-9961 GA-9971
Ifarahan Translucent
Williamplasticity 120 130 150 170 180
Lile ( ShoreA) 30 40 50 60 70
Ìwúwo (g/cm3) 1.1 1.11 1.12 1.14 1.16
Agbara fifẹ (MPa) 6 6 6 6 6.5
Ilọsiwaju(%) 800 500 250 200 150
Agbara omije (kN/m) 15 15 15 15 15
175 'C x22h Ṣeto funmorawon(%) 15 10 8 8 10


Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ kiakia

Awọn ọja WA

IBI IWIFUNNI

Fi kun: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tẹli / WhatsApp / Skype: +86 15221953351
Aṣẹ-lori-ara     2023 Shanghai Herchy Rubber Co., Ltd. Maapu aaye |   Asiri Afihan | Atilẹyin Nipasẹ Leadong.