GA-99X1 Low Compression Set Silicone Rubber (HCR)

Chishandiso: chakakodzera kugadzirwa kwemhete yekuisa chisimbiso, machira, auto zvikamu uye zvimwe zvigadzirwa.
Chinhu chakakosha: kusimba kwepamusoro, kudzika kwakadzika kweseti, isina-chepfu isina kuravira HSE, pfuura kusimbiswa kweRoHS, REACH uye FDA.
  • GA-99X1

  • Herchy

Kuwanikwa:
Huwandu:

Muedzo: 1% yekurapa mumiriri (50% paste yeDBPMH mune silicone gum), 175心5minx 15MPa.


Product parameters
Product GA-9931 GA-9941 GA-9951 GA-9961 GA-9971
Chitarisiko Translucent
Williamplasticity 120 130 150 170 180
Kuoma (ShoreA) 30 40 50 60 70
Density(g/cm3) 1.1 1.11 1.12 1.14 1.16
Tensile simba (MPa) 6 6 6 6 6.5
Elongation(%) 800 500 250 200 150
Simba rekubvarura (kN/m) 15 15 15 15 15
175'C x22h Compression Set(%) 15 10 8 8 10


Zvakapfuura: 
Zvinotevera: 

KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.