GA-99X1 Low Compression Set Silicone Rubber (HCR)

Kopo: e loketse tlhahiso ea lesale la ho tiisa, libethe, likarolo tsa koloi le lihlahisoa tse ling.
Karolo ea bohlokoa: ho tiea ho hoholo, sete e tlase ea khatello, HSE e senang chefo e se nang chefo, e fetisa netefatso ea RoHS, REACH le FDA.
  • GA-99X1

  • Herchy

Boteng:
Bongata:

Teko: 1% ea moemeli oa pheko (50% peista ea DBPMH ka har'a marenene a silicone), 175心5minx 15MPa.


Lihlahisoa tsa lihlahisoa
Sehlahisoa GA-9931 GA-9941 GA-9951 GA-9961 GA-9971
Ponahalo Translucent
Williamplasticity 120 130 150 170 180
Ho thatafala (LebopoA) 30 40 50 60 70
Boima ba 'mele(g/cm3) 1.1 1.11 1.12 1.14 1.16
Tensile Matla (MPa) 6 6 6 6 6.5
Elongation(%) 800 500 250 200 150
Matla a ho lla (kN/m) 15 15 15 15 15
175'C x22h Compression Set(%) 15 10 8 8 10


E fetileng: 
E 'ngoe: 

LIEKETSENG POTLAKO

LIHLAHISO TSA RONA

MOKHOA OA PUISANO

Eketsa: No.33, Lane 159, Taiye Road, Setereke sa Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sebaka sa marang-rang |   Leano la Lekunutu | Tšehetso Ka Leadong.