GA-99X1 Ƙarƙashin Matsi Saitin Silicone Rubber (HCR)

Aikace-aikace: dace da samar da sealing zobe, gadaje, auto sassa da sauran kayayyakin.
Maɓalli mai mahimmanci: babban juriya, ƙananan saiti na matsawa, HSE maras ɗanɗano mai guba, ƙaddamar da amincin RoHS, REACH da FDA.
  • GA-99X1

  • Herchy

samuwa:
Yawan:

Gwaji: 1% na wakili mai warkarwa (manna 50% na DBPMH a cikin silicone danko), 175心5minx 15MPa.


Siffofin samfur
Samfura GA-9931 GA-9941 GA-9951 GA-9961 GA-9971
Bayyanar Translucent
Williamplasticity 120 130 150 170 180
Hardness (ShoreA) 30 40 50 60 70
Girma (g/cm3) 1.1 1.11 1.12 1.14 1.16
Ƙarfin ɗaure (MPa) 6 6 6 6 6.5
Tsawaita(%) 800 500 250 200 150
Ƙarfin hawaye (kN/m) 15 15 15 15 15
175 'C x22h Saitin Matsi (%) 15 10 8 8 10


Na baya: 
Na gaba: 

SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.