GA-99X1 Set de compression basse silicone caoutchouc (HCR) .

A kɛcogo: a bɛnnen don sigilan bololanɛgɛ, dilanw, mobili yɔrɔw ani fɛn wɛrɛw dilanni ma.
Fɛn min ye fɛnba ye: a bɛ se ka muɲu kosɛbɛ, a bɛ se ka degun kosɛbɛ, HSE min tɛ baga ye, a tɛ diya, a bɛ tɛmɛ RoHS, REACH ani FDA ka tiɲɛni kan.
  • GA-99X1 ye

  • Herchy .

A sɔrɔli:
Hakɛ: .

Kɔrɔbɔli : kɛnɛyaji 1% (DBPMH 50% paste silikɔni gomu kɔnɔ), 175心5minx 15MPa.


Product Paramɛtɛrɛw .
Ka kɛ GA-9931 ye GA-9941 ye GA-9951 ye GA-9961 ye GA-9971 ye
Yecogo Translucent .
Williamplasticity (Wiliamplasticité) ye 120 130 150 170 180
Gɛlɛya (Shoaa) . 30 40 50 60 70
Densité(g/cm3) ye. 1.1 1.11 1.12 1.14 1.16
Sɛgɛsɛgɛli fanga (MPa) . 6 6 6 6 6.5
Janya(%) . 800 500 250 200 150
Ɲɛjibɔ fanga (KN/M) . 15 15 15 15 15
175'C x22h Degun Set(%) 15 10 8 8 10


Tɛmɛnen: 
Nata: 

LINKS TELIKANW

An ka fɛn dilannenw .

KUNNAFONIW MINNU BƐ SƆRƆ

A farala: No.33, Lane 159, Taiye sira kan, Fengxian mara la, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Hakilila-jɔ-sɛbɛn     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap (yɔrɔ karti). |   Kunnafoni dogolenw ka sariya | Dɛmɛn By Leadong ye.