GA-99X1 Gucisha make Gushiraho Rubic Silicone (HCR)

Gusaba: bikwiranye no gukora impeta ya kashe, cots, ibice byimodoka nibindi bicuruzwa.
Ikintu cyingenzi: kwihangana cyane, kwikuramo hasi, gushiraho uburozi butagira uburozi HSE, unyuze kuri RoHS, REACH na FDA.
  • GA-99X1

  • Herchy

Kuboneka:
Umubare:

Ikizamini: 1% yumuti ukiza (50% paste ya DBPMH mumase ya silicone), 175 心 5minx 15MPa.


Ibipimo byibicuruzwa
Ibicuruzwa GA-9931 GA-9941 GA-9951 GA-9961 GA-9971
Kugaragara Birasobanutse
Yamamoto 120 130 150 170 180
Gukomera (ShoreA) 30 40 50 60 70
Ubucucike (g / cm3) 1.1 1.11 1.12 1.14 1.16
Imbaraga zingana (MPa) 6 6 6 6 6.5
Kurambura (%) 800 500 250 200 150
Amarira amarira (kN / m) 15 15 15 15 15
175 'C x22h Gushiraho Gushiraho (%) 15 10 8 8 10


Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.