GA-99X1 na ɛwɔ hɔ
Herchy a ɔyɛ ɔbarima
| Nea Ɛwɔ Hɔ: | |
|---|---|
| Dodow: | |
Sɔhwɛ: 1% a ɛyɛ aduru a wɔde sa yare (50% a wɔde DBPMH a wɔde ahyɛ silicone gum mu), 175心5minx 15MPa.
| Nneɛma a wɔyɛ no parameters | |||||
| Adwadeɛ | GA-9931 na ɛwɔ hɔ | GA-9941 na ɛwɔ hɔ | GA-9951 na ɛwɔ hɔ | GA-9961 na ɛwɔ hɔ | GA-9971 na ɛwɔ hɔ |
| Mmaeɛ | Ɛyɛ nea ɛyɛ translucent | ||||
| Williamplasticity a wɔde yɛ nneɛma | 120 | 130 | 150 | 170 | 180 |
| Nneɛma a ɛyɛ den (ShoreA) . | 30 | 40 | 50 | 60 | 70 |
| Nsuo a ɛyɛ den(g/cm3) . | 1.1 | 1.11 | 1.12 | 1.14 | 1.16 |
| Ahoɔden a wɔde twe ade (MPa) . | 6 | 6 | 6 | 6 | 6.5 |
| Ntrɛwmu(%) . | 800 | 500 | 250 | 200 | 150 |
| Ahoɔden a ɛtetew mu (kN/m) . | 15 | 15 | 15 | 15 | 15 |
| 175'C x22h Nhyɛso Set (%) . | 15 | 10 | 8 | 8 | 10 |