GA-99X1 Hoʻopaʻa haʻahaʻa hoʻopaʻa haʻahaʻa Silicone Rubber (HCR)

Noi: kūpono no ka hana ʻana i ke apo sealing, cots, ʻāpana kaʻa a me nā huahana ʻē aʻe.
ʻO ka hiʻohiʻona koʻikoʻi: ke kūpaʻa kiʻekiʻe, ka hoʻonohonoho haʻahaʻa haʻahaʻa, ka HSE ʻono ʻole ʻawaʻawa, e hele i ka hōʻoia o RoHS, REACH a me FDA.
  • GA-99X1

  • Herchy

Loaʻa:
Nui:

Ho'āʻo: 1% o ka lāʻau lapaʻau (50% paʻi o DBPMH i ka silicone gum), 175心5minx 15MPa.


Nā palena huahana
Huahana GA-9931 GA-9941 GA-9951 GA-9961 GA-9971
Ka nana aku Alohilohi
Williamplasticity 120 130 150 170 180
Paʻakikī (ShoreA) 30 40 50 60 70
Māmā (g/cm3) 1.1 1.11 1.12 1.14 1.16
Ka ikaika uʻi (MPa) 6 6 6 6 6.5
Elongation(%) 800 500 250 200 150
Kaha waimaka (kN/m) 15 15 15 15 15
175'C x22h Hoʻonohonoho hoʻoemi (%) 15 10 8 8 10


Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.