GA-60X1F Ultra Heat-resistant Silicone Rubber ((300℃) (HCR)
Application: suitable for producing auto parts, heat-resistant cots, heat-resistantseals and other products.
Key features: good heat resistanceand mechanical strength, pass theauthentication of RoHS, REACH, and FDA.
Test: 1% of curing agent (50% paste of DBPMH in silicone gum),175°C x 5min x 15MPa。
| 300 degree Product parameters | |||||
| Product | GA-6041F | GA-6051F | GA-6061F | GA-6071F | |
| Appearance | Beige | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Hardness (ShoreA) | 40 | 50 | 60 | 70 | |
| Density(g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Tensile strength (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Elongation(%) | 700 | 600 | 500 | 400 | |
| Tear strength (kN/m) | 15 | 20 | 25 | 25 | |
| air ageing 300℃ x70H | Hardness | 46 | 63 | 73 | 77 |
| Tension strength | 5.2 | 5.0 | 4.9 | 5.2 | |
| Elongation | 350.0 | 220.0 | 180.0 | 160.0 | |