GA-60X1F Mpira wa Silicone unaostahimili Joto (((300℃)) (HCR)
Maombi: yanafaa kwa ajili ya kuzalisha sehemu za magari, vitanda vinavyostahimili joto, vizuia joto na bidhaa nyingine.
Vipengele muhimu: upinzani mzuri wa joto na nguvu ya mitambo, kupitisha uthibitishaji wa RoHS, REACH, na FDA.
Jaribio: 1% ya dawa ya kuponya (50% ya kuweka DBPMH kwenye gum ya silicone), 175°C x 5min x 15MPa.
| Vigezo vya bidhaa vya digrii 300 | |||||
| Bidhaa | GA-6041F | GA-6051F | GA-6061F | GA-6071F | |
| Muonekano | Beige | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Ugumu (ShoreA) | 40 | 50 | 60 | 70 | |
| Msongamano(g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Nguvu ya mkazo (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Kurefusha(%) | 700 | 600 | 500 | 400 | |
| Nguvu ya machozi (kN/m) | 15 | 20 | 25 | 25 | |
| hewa kuzeeka 300℃ x70H | Ugumu | 46 | 63 | 73 | 77 |
| Nguvu ya mvutano | 5.2 | 5.0 | 4.9 | 5.2 | |
| Kurefusha | 350.0 | 220.0 | 180.0 | 160.0 | |