GA-60X1F Ultra Kulayl u adkaysta Silikoon Rubber (300 ℃) (HCR)

GA-60X1F Caag Silikoon u adkaysta kulaylka ((300℃) (HCR)
Codsiga: ku habboon soo saarista qaybaha baabuurta, sariiraha kulaylka u adkaysta, shaabada kulaylka iyo alaabada kale.
Astaamaha muhiimka ah: caabbinta kulaylka wanaagsan iyo xoogga farsamada, gudbi xaqiijinta RoHS, REACH, iyo FDA.
  • GA-60X1F

  • Herchy

Helitaanka:
Tirada:

GA-60X1F Caag Silikoon u adkaysta kulaylka ((300℃) (HCR)


Codsiga: ku habboon soo saarista qaybaha baabuurta, sariiraha kulaylka u adkaysta, shaabada kulaylka iyo alaabada kale.
Astaamaha muhiimka ah: caabbinta kulaylka wanaagsan iyo xoogga farsamada, gudbi xaqiijinta RoHS, REACH, iyo FDA.
Tijaabada: 1% ee wakiilka daawaynta (50% koollada DBPMH ee xanjada silikoonka),175°C x 5min x 15MPa.


300 darajo Alaabta
Alaabta GA-6041F GA-6051F GA-6061F GA-6071F
Muuqashada Beige
Williamplasticity 150 200 240 240
Adag ( ShoreA) 40 50 60 70
Cufnaanta (g/cm3) 1.14 1.16 1.18 1.2
Xoog xajin (MPa) 8.5 9 9.5 9
Dheeraynta(%) 700 600 500 400
Xoogga jeexjeexa (kN/m) 15 20 25 25
hawada gabowga 300 ℃ x70H Adag 46 63 73 77
Xoogga kacsanaanta 5.2 5.0 4.9 5.2
Dheeraynta 350.0 220.0 180.0 160.0


Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.