GA-60X1F Ultra Heat-repugnans Silicone Purgamentum (300℃)(HCR)

GA-60X1F Ultra Heat resistens Silicone Purgamentum ((300℃) (HCR)
Applicatio: apta ad producendas partes autocineticas, calor resistentes casas, calor resistentes et alia producta.
Key lineamenta: bonus calor resistens et vires mechanicae, theauthenticationem RoHS, SPATIUM, FDA transmittunt.
  • GA-60X1F

  • Herchy

Availability:
Quantity:

GA-60X1F Ultra Heat resistens Silicone Purgamentum ((300℃) (HCR)


Applicatio: apta ad producendas partes autocineticas, calor resistentes casas, calor resistentes et alia producta.
Key lineamenta: bonus calor resistens et vires mechanicae, theauthenticationem RoHS, SPATIUM, FDA transmittunt.
Test: 1% curationis agentis (50% crustulum DBPMH in gummi siliconis), 175°C x 5min x 15MPa。


CCC gradum Product parametri
Productum GA-6041F GA-6051F GA-6061F GA-6071F
Aspectus Beige
Williamplasticity 150 200 240 240
Duritia (ShoreA) 40 50 60 70
Densitas (g/cm3) 1.14 1.16 1.18 1.2
Roboris distrahentes (MPa) 8.5 9 9.5 9
Prolongatio(%) 700 600 500 400
Robur scindere (kN/m) 15 20 25 25
aeris senescentis 300℃ x70H duritia 46 63 73 77
Tensio vires 5.2 5.0 4.9 5.2
Prolongatio 350.0 220.0 180.0 160.0


Priora: 
Next: 

ORIGINAL LINKS

Our Products

Contact Information

Add: No.33, Lane CLIX, Taiye via, Fengxian District, Shanghai
Tel / whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Flexilis Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.