Prawf: 1% o asiant halltu (50% past o DBPMH mewn gwm silicon), 175 ° C x 5 munud x 15MPa.
| Paramedrau Cynnyrch 300 gradd | |||||
| Cynnyrch | GA-6041F | GA-6051F | GA-6061F | GA-6071F | |
| Ymddangosiad | llwydfelyn | ||||
| Williamplastigedd | 150 | 200 | 240 | 240 | |
| Caledwch (ShoreA) | 40 | 50 | 60 | 70 | |
| Dwysedd(g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Cryfder tynnol (MPa) | 8.5 | 9 | 9.5 | 9 | |
| elongation(%) | 700 | 600 | 500 | 400 | |
| Cryfder dagrau (kN/m) | 15 | 20 | 25 | 25 | |
| aer yn heneiddio 300 ℃ x70H | Caledwch | 46 | 63 | 73 | 77 |
| Cryfder tensiwn | 5.2 | 5.0 | 4.9 | 5.2 | |
| Elongation | 350.0 | 220.0 | 180.0 | 160.0 | |