GA-60X1F Kawotchou Silikon ultra reziste chalè ((300℃) (HCR)
Aplikasyon: apwopriye pou pwodwi pati oto, kabann ki reziste chalè, sele ki reziste chalè ak lòt pwodwi.
Karakteristik kle: bon rezistans chalè ak fòs mekanik, pase otantifikasyon RoHS, REACH, ak FDA.
Tès: 1% nan ajan geri (50% keratin nan DBPMH nan jansiv silikon), 175 ° C x 5 min x 15MPa.
| 300 degre pwodwi paramèt | |||||
| Pwodwi | GA-6041F | GA-6051F | GA-6061F | GA-6071F | |
| Aparans | Bèj | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Dite (ShoreA) | 40 | 50 | 60 | 70 | |
| Dansite (g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Fòs rupture (MPa) | 8.5 | 9 | 9.5 | 9 | |
| elongasyon (%) | 700 | 600 | 500 | 400 | |
| Fòs chire (kN/m) | 15 | 20 | 25 | 25 | |
| lè aje 300℃ x70H | Dite | 46 | 63 | 73 | 77 |
| Fòs tansyon | 5.2 | 5.0 | 4.9 | 5.2 | |
| Elongasyon | 350.0 | 220.0 | 180.0 | 160.0 | |