GA-60X1F Ultra Okpomọkụ silicone rọba ((300℃) (HCR)
Ngwa: adabara maka imepụta akụkụ akpaaka, akwa ndị na-ekpo ọkụ na-ekpo ọkụ, mkpuchi okpomọkụ na ngwaahịa ndị ọzọ.
Njirimara ndị dị mkpa: ezigbo nguzogide okpomọkụ na ike igwe, gafere nkwenye nke RoHS, REACH, na FDA.
Nnwale: 1% nke onye na-agwọ ọrịa (50% tapawa DBPMH na silicone gum), 175°C x 5min x 15MPa.
| 300 ogo Product parameters | |||||
| Ngwaahịa | GA-6041F | GA-6051F | GA-6061F | GA-6071F | |
| Ọdịdị | Agba aja aja | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Isi ike (ShoreA) | 40 | 50 | 60 | 70 | |
| Njupụta (g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Ike tensile (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Mgbatị(%) | 700 | 600 | 500 | 400 | |
| Ike akwa mmiri (kN/m) | 15 | 20 | 25 | 25 | |
| ikuku ịka nká 300 ℃ x70H | Isi ike | 46 | 63 | 73 | 77 |
| Ike erughị ala | 5.2 | 5.0 | 4.9 | 5.2 | |
| Ogologo oge | 350.0 | 220.0 | 180.0 | 160.0 | |