GA-60X1F
Herchy
| Kuwanikwa: | |
|---|---|
| Huwandu: | |
GA-60X1F Ultra Heat-resistant Silicone Rubber ((300℃) (HCR)
Chishandiso: chakakodzera kugadzira zvikamu zvemotokari, machira anodzivirira kupisa, anodzivirira kupisa uye zvimwe zvigadzirwa.
Akakosha maficha: yakanaka kupisa kupisa uye simba remuchina, pfuura kusimbiswa kweRoHS, REACH, uye FDA.
Muedzo: 1% yekurapa mumiririri (50% paste yeDBPMH mune silicone gum), 175 ° C x 5min x 15MPa.
| 300 degree Chigadzirwa parameters | |||||
| Product | GA-6041F | GA-6051F | GA-6061F | GA-6071F | |
| Chitarisiko | Beige | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Kuoma (ShoreA) | 40 | 50 | 60 | 70 | |
| Density(g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Tensile simba (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Elongation(%) | 700 | 600 | 500 | 400 | |
| Simba rekubvarura (kN/m) | 15 | 20 | 25 | 25 | |
| mhepo kuchembera 300 ℃ x70H | Kuoma | 46 | 63 | 73 | 77 |
| Tension simba | 5.2 | 5.0 | 4.9 | 5.2 | |
| Elongation | 350.0 | 220.0 | 180.0 | 160.0 | |