I-GA-60X1F
I-Herchy
| Ukutholakala: | |
|---|---|
| Ubuningi: | |
I-GA-60X1F Irabha Ye-Silicone Ekwazi ukumelana nokushisa ((300℃) (HCR)
Isicelo: ilungele ukukhiqiza izingxenye zezimoto, amacansi amelana nokushisa, ukumelana nokushisa neminye imikhiqizo.
Izici ezibalulekile: ukumelana nokushisa okuhle namandla emishini, dlula ukuqinisekiswa kwe-RoHS, REACH, kanye ne-FDA.
Isivivinyo: 1% we-ejenti yokwelapha (50% unamathisele we-DBPMH ku-silicone gum), 175°C x 5min x 15MPa.
| Amapharamitha womkhiqizo angama-300 degree | |||||
| Umkhiqizo | I-GA-6041F | I-GA-6051F | I-GA-6061F | I-GA-6071F | |
| Ukubukeka | Beige | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Ukuqina (ShoreA) | 40 | 50 | 60 | 70 | |
| Ukuminyana(g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Amandla e-Tensile (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Ubude(%) | 700 | 600 | 500 | 400 | |
| Amandla wezinyembezi (kN/m) | 15 | 20 | 25 | 25 | |
| umoya ukuguga 300℃ x70H | Ukuqina | 46 | 63 | 73 | 77 |
| Amandla okuqina | 5.2 | 5.0 | 4.9 | 5.2 | |
| Ukwelula | 350.0 | 220.0 | 180.0 | 160.0 | |