GA-60X1F
Herchy
| kupezeka: | |
|---|---|
| kuchuluka: | |
GA-60X1F Ultra Heat-resistant Silicone Rubber (((300℃) (HCR)
Kugwiritsa ntchito: koyenera kupanga zida zamagalimoto, machira osagwira kutentha, zoletsa kutentha ndi zinthu zina.
Zofunika kwambiri: kukana kutentha kwabwino komanso mphamvu zamakina, kupititsa kutsimikizika kwa RoHS, REACH, ndi FDA.
Kuyesa: 1% ya machiritso (50% phala la DBPMH mu chingamu cha silicone), 175 ° C x 5min x 15MPa.
| 300 digiri Zogulitsa magawo | |||||
| Zogulitsa | Mtengo wa GA-6041F | Mtengo wa GA-6051F | Mtengo wa GA-6061F | Mtengo wa GA-6071F | |
| Maonekedwe | Beige | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Kuuma (ShoreA) | 40 | 50 | 60 | 70 | |
| Kachulukidwe (g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Mphamvu yamagetsi (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Kutalikira (%) | 700 | 600 | 500 | 400 | |
| Mphamvu yamisozi (kN/m) | 15 | 20 | 25 | 25 | |
| mpweya kukalamba 300 ℃ x70H | Kuuma | 46 | 63 | 73 | 77 |
| Mphamvu yamphamvu | 5.2 | 5.0 | 4.9 | 5.2 | |
| Elongation | 350.0 | 220.0 | 180.0 | 160.0 | |