GA-60X1A
Herchy
| Availability: | |
|---|---|
| Quantity: | |
GA-60X1A Heat-resistant Silicone Rubber (250 And 300 OC) (HCR)
Application: suitable for producing auto parts, heat-resistant cots, heat-resistantseals and other products.
Key features: good heat resistanceand mechanical strength, pass theauthentication of RoHS, REACH, and FDA.
Test: 1% of curing agent (50% paste of DBPMH in silicone gum),175°C x 5min x 15MPa。
| 250 degree Product parameters | |||||
| Product | GA-6041A | GA-6051A | GA-6061A | GA-6071A | |
| Appearance | Translucent | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Hardness (ShoreA) | 40 | 50 | 60 | 70 | |
| Density(g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Tensile strength (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Elongation(%) | 700 | 600 | 500 | 400 | |
| Tear strength (kN/m) | 15 | 20 | 25 | 25 | |
| air ageing 250℃ x70H | Hardness | 45 | 54 | 64 | 75 |
| Tension strength | 6.2 | 7.3 | 7.5 | 6.5 | |
| Elongation | 380.0 | 300.0 | 280.0 | 200.0 | |