FV9200
Herchi
| Mavjudligi: | |
|---|---|
| Miqdori: | |
Elementlar |
Ko'rsatkichlar |
|||
Baholar |
FV9240 |
FV9250 |
FV9260 |
|
Sinov usullari / Tashqi ko'rinish |
Sutli oq shaffof |
|||
O'ziga xos tortishish / g / sm3 |
ASTM D792 |
1.42 |
1.44 |
1.45 |
Qattiqlik / qirg'oqA |
ASTM D2240 |
40 |
50 |
60 |
Kuchlanish kuchi/MPa |
ASTM D412 |
10.1 |
10.2 |
10.3 |
Uzilishdagi cho'zilish /% |
ASTM D412 |
490 |
457 |
440 |
Yirtilish kuchi/KN/m |
ASTM D624-B |
35 |
42 |
43 |
Siqish to'plami (177 ℃ * 22 soat) |
ASTM D395 |
11 |
11 |
12 |
* Issiqlikka qarshilik |
Qattiqlikning o'zgarishi / qirg'oq A |
+3 |
+3 |
+2 |
Kuchlanish kuchi o'zgarishi, % |
-19 |
-16 |
-17 |
|
Uzilishdagi cho'zilish o'zgarishi, % |
-14 |
-17 |
-18 |
|
Yoqilg'i C Ovoz balandligi/% 23℃/72 soat |
ASTM D471 |
23 |
21 |
20 |
Qattiqlashuv holati |
0,7 DBPH, Bosish bilan davolash: 170 ℃ × 15 min , Davolanishdan keyingi: 200 ℃ × 4 soat |
|||
Tavsiya etilgan harakatlar:
Vulkanizatsiya uchun bisdipenta kimyoviy agentining 0,6 dan 1 qismigacha (2,5-dimetil-2,5-bis (tert-butilperoksi) geksan) foydalanish tavsiya etiladi.
Mijozlar mahsulotning o'lchami va quritish usulidan kelib chiqib, eng mos harorat va vaqtni tanlashlari kerak.
Mahsulot qadoqlash:
Ushbu mahsulot xavfli emas, uning o'rniga karton, plastmassa va har bir sumka uchun 10 kilogramm, har bir qutiga 2 ta qopdan iborat.
Saqlash muddati:
Ushbu mahsulot sovuq oqim qobiliyatiga ega, tashish yoki foydalanish paytida uni shikastlamaslik uchun sumkadan qochish kerak.
Salqin, quruq muhitda saqlash muddati 12 oy.