Zinc oxide wani fili ne na sinadarai tare da dabarar ZnO. A zahiri baya narkewa a cikin ruwa kuma yana narkewa a cikin duka acid da tushe mai ƙarfi. Zinc oxide shine babban ƙari na inorganic wanda aka yi amfani da shi sosai a cikin samar da roba na roba. Ana amfani da ZnO don samar da ko dai na halitta/Synthetic roba & latex a cikin Rubber ko Cable Industries. Ana amfani dashi a cikin waɗannan aikace-aikacen azaman wakili mai vulcanizing, wakili mai ƙarfafawa da kuma wakili mai canza launi don ƙyale robar ya mallaki juriya mai lalata, juriya mai tsage & elasticity. Hakanan ana amfani dashi azaman wakili mai canza launi da filler don Farin Rubber, azaman wakili mai ɓarna don Neoprene Rubber, da kuma azaman mai daidaita haske don ɓangarorin filasta mai kyau kamar polyolefins ko PVC. Herchy Rubber yana ba da nau'ikan zaɓi na makin zinc oxide don saduwa da buƙatu daban-dabanZinc oxide-ZnO
Zinc oxide wani abu ne na inorganic tare da tsarin sinadaran ZnO, oxide na zinc. Ba shi da narkewa a cikin ruwa kuma yana narkewa a cikin acid da tushe mai ƙarfi. Zinc oxide abu ne na sinadaran gama gari kuma ana amfani dashi sosai a cikin roba.
ZnO da ake amfani da matsayin vulcanizing aiki wakili, ƙarfafa wakili da canza launi wakili na halitta roba, roba roba da latex a cikin roba ko na USB masana'antu masana'antu don yin roba da kyau lalata juriya, hawaye juriya da kuma elasticity. Ana amfani dashi azaman wakili mai canza launi da mai filler farin roba, wakili mai ɓoyewa a cikin roba neoprene da mai daidaita haske na robobi kamar polyolefin ko polyvinyl chloride don barbashi mai kyau (kimanin 0.1μm a girman).
Herchy Rubber yana da nau'ikan nau'ikan nau'ikan zinc oxide don zaɓar don buƙatu iri-iri
| Herchy | Abun ciki na Znic oxide | Abun ciki mai aiki na Znic oxide | Pb2+ Abubuwan ciki | Cu2+ abun ciki | Mn2+ Abubuwan ciki | Takamammen yanki na farfajiya | yawa | PH | Sieve ragowar (45μm) | Aikace-aikace |
| daraja | wt% | wt% | wt% | wt% | wt% | m2/g | g/cm3 | % | ||
| NC105 | min.54 | min.93 | max.0.001 | max. 0.0005 | max.0.001 | 20-30 | 3.6 | Tayoyi, Bututun ciki, Rollers, Conveyor belts, Auto sassa, Takalmi | ||
| NC205 | min.50 | min.93 | max.0.001 | max. 0.0005 | max.0.001 | 25 | 3.4 | Tayoyin mota, Tayoyin babur, Takalma, Rollers, Conveyor belts, Auto sassa, Roba profiles | ||
| NC232 | min.25 | min.25 | max.0.001 | max.0.001 | max.0.001 | max.0.2 | Tayoyin keke, Kayan mota, zoben roba, Takalmi | |||
| NC234 | 37-43 | max.0.001 | max.0.001 | max.0.001 | 8.5-10.5 | max.0.5 | Tayoyi, Bututun ciki, Rollers, Conveyor belts, Auto sassa, Takalmi | |||
| RA | min.40 | max.0.002 | max.0.001 | max.0.001 | 15 | Takalma tafin kafa, Keke ciki bututu, Keke taya, Motar ciki bututu, Roba sassa, Roba ball | ||||
| NC236 | 60-65 | min.90 | max.0.001 | max. 0.0005 | max.0.001 | 40 | 3.6 | Tayoyi, Bututun ciki, Rollers, Conveyor belts, Auto sassa, Takalmi | ||
| Saukewa: TR809 | 88-93 | max.0.001 | max. 0.0005 | max.0.001 | 40 | 4.6 | Tayoyi, Bututun ciki, Rollers, Conveyor belts, Auto sassa, Takalmi |
1. Taya
Haɓaka haɓakar zafin jiki, juriya, juriya, juriya, ƙarfi da sauran alamun samfur, kuma yana iya adana kusan 30% na adadin zinc oxide.
2. Kayayyakin roba
① Kunna zinc oxide ne yafi amfani da matsayin ƙarfafa wakili na roba don yin roba da kyau lalata juriya, hawaye juriya da elasticity da elongation.
②Ana amfani da shi azaman totur na roba vulcanization tsari kuma shi ne multifunctional roba compounding wakili, yafi amfani da matsayin vulcanization aiki wakili da ƙarfafa wakili na halitta roba, roba roba da kuma latex.
③A matsayin wakili mai aiki na vulcanization, ana rarraba shi daidai a cikin kayan roba, yana da babban yanki mai lamba tare da hydrogen sulfide, kuma yana da babbar dama don aiwatar da halayen tsaka-tsaki, da samfuran zinc oxide masu aiki suna da taimakon abubuwa masu aiki don haɓaka jujjuyawar zinc oxide zuwa zinc sulfide.
④ A matsayin sulfide oxidizer, aikinsa shine don haɓaka aikin haɓakawa, rage yawan adadin kuzari da rage sake zagayowar vulcanization.
⑤Yana iya hanzarta saurin vulcanization, inganta yanayin zafi na roba mai ɓarna, da kuma sa vulcanization ya zama cikakke.
⑥ A cikin masana'antar roba, musamman a cikin samar da samfuran roba na gaskiya, zinc oxide mai aiki shine kyakkyawan wakili mai vulcanizing.
3. roba roba
Ana amfani dashi azaman kunnawa, mai saurin ɓarnawa da wakili mai ƙarfafawa, kuma yana da tasirin canza launi. Inganta vulcanization na roba, kunnawa da ƙarfafawa, tasirin tsufa, na iya ƙarfafa tsarin vulcanization, haɓaka juriya na hawaye da juriya na samfuran roba.