GA-2039M
Herchy
| Ho ba teng: | |
|---|---|
| Bongata: | |
Teko: A/B karo-karolelano ea 1 :1, 130°C x 5min x 15MPa
| Lihlahisoa tsa lihlahisoa | |||||
| Sehlahisoa | GA-2039M | GA-2049M | GA-2059M | GA-2069M | |
| Ponahalo | Translucent | ||||
| Viscosity(Pa.s) |
A:1000 B:2000 |
A:1000 B:2000 |
A:1000 B:2000 |
A:1000 B:2000 |
|
| Ho thatafala (LebopoA) | 30 | 40 | 50 |
60 |
|
| Boima ba 'mele(g/cm3) | 1.13 |
1.12 | 1.12 | 1.14 | |
| Tensile Matla (MPa) | 6 |
6 |
6 |
5 |
|
| Elongation(%) | 600 | 550 | 450 | 350 | |
| Matla a ho lla (kN/m) | 10 | 10 | 15 |
20 | |