GA-2039M
Herchy
| Wātea: | |
|---|---|
| Rahi: | |
Whakamātautau: A/B ōwehenga o 1 :1, 130°C x 5min x 15MPa
| Tawhā hua | |||||
| Hua | GA-2039M | GA-2049M | GA-2059M | GA-2069M | |
| Te ahua | Puatarangi | ||||
| Viscosity(Pa.s) |
A:1000 B:2000 |
A:1000 B:2000 |
A:1000 B:2000 |
A:1000 B:2000 |
|
| Maama (ShoreA) | 30 | 40 | 50 |
60 |
|
| Kiato(g/cm3) | 1.13 |
1.12 | 1.12 | 1.14 | |
| Te kaha o te kaha (MPa) | 6 |
6 |
6 |
5 |
|
| Whakaroa(%) | 600 | 550 | 450 | 350 | |
| Te kaha roimata (kN/m) | 10 | 10 | 15 |
20 | |