GA-2039M
Herchy
| Kupezeka: | |
|---|---|
| Kuchuluka: | |
Kuyesa: A/B chiŵerengero cha 1:1, 130°C x 5min x 15MPa
| Zogulitsa katundu | |||||
| Zogulitsa | GA-2039M | GA-2049M | Mtengo wa GA-2059M | GA-2069M | |
| Maonekedwe | Zowoneka bwino | ||||
| Viscosity (Pa.s) |
A: 1000 B:2000 |
A:1000 B:2000 |
A:1000 B:2000 |
A:1000 B:2000 |
|
| Kuuma (ShoreA) | 30 | 40 | 50 |
60 |
|
| Kachulukidwe (g/cm3) | 1.13 |
1.12 | 1.12 | 1.14 | |
| Mphamvu yamagetsi (MPa) | 6 |
6 |
6 |
5 |
|
| Kutalikira (%) | 600 | 550 | 450 | 350 | |
| Mphamvu yamisozi (kN/m) | 10 | 10 | 15 |
20 | |