FV9502 na ɛwɔ hɔ
Herchy a ɔyɛ ɔbarima
| Nea Ɛwɔ Hɔ: | |
|---|---|
| Dodow: | |
Nneɛma |
Index |
||
Serial nɔma a wɔde di dwuma |
FV9552 na ɛwɔ hɔ |
FV9562 na ɛwɔ hɔ |
|
Mmaeɛ Akwan a Wɔfa so Sɔ Sɔhwɛ |
ɛyɛ kɔkɔɔ |
||
Nneɛma a ɛtwe ade ba fam pɔtee/ g/cm3 |
ASTM D792 na ɛwɔ hɔ |
1.42 |
1.43 |
Nneɛma a ɛyɛ den/mpoanoA |
ASTM D2240 na ɛwɔ hɔ |
52 |
61 |
Tensile Ahoɔden/MPa |
ASTM D412 na ɛwɔ hɔ |
10.2 |
9.4 |
Elongation Wɔ Ahomegye Mu /% . |
ASTM D412 na ɛwɔ hɔ |
330 |
280 |
Nsuo Ahoɔden/KN/m |
ASTM D624-B na ɛwɔ hɔ |
20 |
19 |
Nhyɛso Set (177 ° C * 22h ) . |
ASTM D395 na ɛwɔ hɔ |
7 |
8 |
Nketesie/% |
ASTM D1054 na ɛwɔ hɔ |
35 |
34 |
*Ɔhyew a ɛko tia |
Hardness nsakrae /shore A. Ɛyɛ den sɛ wobɛsesa /shore A |
2 |
2 |
Hardness nsakrae /shore A. Ɛyɛ den sɛ wobɛsesa /shore A |
-24 |
-23 |
|
Elongation wɔ break nsakrae mu, % . |
-21 |
-20 |
|
Fuel C |
ASTM D471 na ɛwɔ hɔ |
22 |
21 |
Tebea a Wɔde Sa Ayaresa |
0.5 afã bis-2-5, ɔfa biako vulcanisation 170°C×15min, ɔfa abien vulcanisation: 200°C×4h |
||
Nneyɛe a wɔkamfo kyerɛ:
Wɔhyɛ nyansa sɛ wɔmfa bisdisulfide (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane) afã horow 0.4-0.7 nni dwuma.
Ɛsɛ sɛ adetɔfo paw ɔhyew ne bere a ɛfata sen biara a wɔde bɛsa yare no gyina aduru no kɛse ne ɔkwan a wɔfa so sa yare no so.
Nneɛma a wɔde kyekyere nneɛma:
Saa ade yi nyɛ asiane, mmom ɛyɛ cardstock, plastic, ne kilogram 10 wɔ bag biara mu, bag 2 wɔ adaka biara mu.
Mfe a wɔde sie:
Saa ade yi wɔ awɔw mu nsu a ɛsen, ɛsɛ sɛ wɔkwati bag no sɛnea ɛbɛyɛ a ɛrensɛe bere a wɔde rekɔ anaasɛ wɔde redi dwuma no.
Fa sie baabi a ɛhɔ yɛ nwini na ɛhɔ yɛ kusuu a ɛtra hɔ asram 12.