FV9502
Herchy
Beskikberens: | |
---|---|
kwantiteit: | |
Items |
Yndeks |
||
Searynûmer |
Fv9552 |
FV9562 |
|
Ferskining Testmethoden |
gielich |
||
Spesifike swiertekrêft / G / CM3 |
ASTM D792 |
1.42 |
1.43 |
Hardness / Shorea |
ASTM D2240 |
52 |
61 |
Tensile sterkte / MPA |
ASTM D412 |
10.2 |
9.4 |
ELONGATION BY BREAK /% |
ASTM D412 |
330 |
280 |
Trienter sterkte / kn / m |
ASTM D624-B |
20 |
19 |
Kompresje Set (177 ℃ * 22) |
ASTM D395 |
7 |
8 |
Fresalience /% |
ASTM D1054 |
35 |
34 |
* Heat fersets |
Hardheid feroarje / wâl a |
2 |
2 |
Hardheid feroarje / wâl a |
-24 |
-23 |
|
ELONGATION OP BREAK WIJZE,% |
-21 |
-20 |
|
Fuel C |
ASTM D471 |
22 |
21 |
Genêzen tastân |
0,5 dielen fan BIS-2-5, ien etappe Vulcanisaasje 170 ℃ × 15min, twa etappe Vulcanisaasje: 200 ℃ × 4h |
Oanbefellende aksjes:
It is suggerearre om 0,4-0,7 dielen fan BISDISULUSCED te brûken (2,5-DIMETHYL-2,5-BIS (Tert-Butylperoxy) Hexane).
Klanten moatte de meast geskikte temperatuer en tiid kieze foar genêzen op basis fan 'e grutte fan it produkt en metoade foar genêzen.
Produkt ferpakking:
Dit produkt is net gefaarlik, it is ynstee gearstald út Cardstock, plestik, en 10 kilogram per tas, 2 tassen per fak.
Age of Storage:
Dit produkt hat in kâlde streamkapasiteit, de tas moat wurde foarkommen wurde om it net te beskeadige tidens ferfier of utilisaasje.
Hâld op in koele, droege omjouwing mei in shelf libben fan 12 moannen.
Items |
Yndeks |
||
Searynûmer |
Fv9552 |
FV9562 |
|
Ferskining Testmethoden |
gielich |
||
Spesifike swiertekrêft / G / CM3 |
ASTM D792 |
1.42 |
1.43 |
Hardness / Shorea |
ASTM D2240 |
52 |
61 |
Tensile sterkte / MPA |
ASTM D412 |
10.2 |
9.4 |
ELONGATION BY BREAK /% |
ASTM D412 |
330 |
280 |
Trienter sterkte / kn / m |
ASTM D624-B |
20 |
19 |
Kompresje Set (177 ℃ * 22) |
ASTM D395 |
7 |
8 |
Fresalience /% |
ASTM D1054 |
35 |
34 |
* Heat fersets |
Hardheid feroarje / wâl a |
2 |
2 |
Hardheid feroarje / wâl a |
-24 |
-23 |
|
ELONGATION OP BREAK WIJZE,% |
-21 |
-20 |
|
Fuel C |
ASTM D471 |
22 |
21 |
Genêzen tastân |
0,5 dielen fan BIS-2-5, ien etappe Vulcanisaasje 170 ℃ × 15min, twa etappe Vulcanisaasje: 200 ℃ × 4h |
Oanbefellende aksjes:
It is suggerearre om 0,4-0,7 dielen fan BISDISULUSCED te brûken (2,5-DIMETHYL-2,5-BIS (Tert-Butylperoxy) Hexane).
Klanten moatte de meast geskikte temperatuer en tiid kieze foar genêzen op basis fan 'e grutte fan it produkt en metoade foar genêzen.
Produkt ferpakking:
Dit produkt is net gefaarlik, it is ynstee gearstald út Cardstock, plestik, en 10 kilogram per tas, 2 tassen per fak.
Age of Storage:
Dit produkt hat in kâlde streamkapasiteit, de tas moat wurde foarkommen wurde om it net te beskeadige tidens ferfier of utilisaasje.
Hâld op in koele, droege omjouwing mei in shelf libben fan 12 moannen.