Fv9502
Chapakati
Kupezeka: | |
---|---|
Kuchuluka: | |
Chinthu | Mapeto | ||
Nambala ya siriyo | Fv95522 | Fv9562 | |
Kaonekedwe Njira Zoyeserera | chikasu | ||
Mphamvu zapadera / g / cm3 | Astm D792 | 1.42 | 1.43 |
Kuvuta / shoreya | ASMM D2240 | 52 | 61 |
Kukhala mphamvu / MPA | Astm D412 | 10.2 | 9.4 |
Elongition ku Break /% | Astm D412 | 330 | 280 |
Vyotsani mphamvu / k / m | Astm D624-B | 20 | 19 |
Kuphatikizika kwa malo (177 ℃ * 22h) | Astm D395 | 7 | 8 |
Kukhazikika /% | ASMM D1054 | 35 | 34 |
* Kukana kutentha | Kusintha kwamphamvu / gombe la | 2 | 2 |
Kusintha kwamphamvu / gombe la | -24 | -23 | |
Elongsition pakasintha,% | -21 | -20 | |
Mafuta C | Astm D471 | 22 | 21 |
Kuchirikiza | Magawo 0,5 a Bis-2-5, gawo limodzi gawo limodzi la 170 ℃ ℃ |
Zochita Zofunika:
Ikufotokozerani magwiridwe a 0,4-0.7 a Bisdisilfide (2,5-dimethyl-2,5-Bis (Tert-Butylperoxy) Hexane).
Makasitomala ayenera kusankha kutentha koyenera komanso nthawi yochiritsa kukula kwa kukula kwa malonda ndi njira yochiritsa.
Paketi Yogulitsa:
Izi sizowopsa, zimakhala m'malo mwa kadi kaditoni, pulasitiki, ma kilogalamu 10 pa thumba, matumba awiri pabokosi.
Zaka zosungirako:
Izi zimapangitsa kuti pakhale kuzizira, thumba liyenera kupewedwa kuti lisawonongeke poyendetsa kapena kugwiritsa ntchito.
Khalani m'malo ozizira, owuma ndi moyo wa alumali miyezi 12.
Chinthu | Mapeto | ||
Nambala ya siriyo | Fv95522 | Fv9562 | |
Kaonekedwe Njira Zoyeserera | chikasu | ||
Mphamvu zapadera / g / cm3 | Astm D792 | 1.42 | 1.43 |
Kuvuta / shoreya | ASMM D2240 | 52 | 61 |
Kukhala mphamvu / MPA | Astm D412 | 10.2 | 9.4 |
Elongition ku Break /% | Astm D412 | 330 | 280 |
Vyotsani mphamvu / k / m | Astm D624-B | 20 | 19 |
Kuphatikizika kwa malo (177 ℃ * 22h) | Astm D395 | 7 | 8 |
Kukhazikika /% | ASMM D1054 | 35 | 34 |
* Kukana kutentha | Kusintha kwamphamvu / gombe la | 2 | 2 |
Kusintha kwamphamvu / gombe la | -24 | -23 | |
Elongsition pakasintha,% | -21 | -20 | |
Mafuta C | Astm D471 | 22 | 21 |
Kuchirikiza | Magawo 0,5 a Bis-2-5, gawo limodzi gawo limodzi la 170 ℃ ℃ |
Zochita Zofunika:
Ikufotokozerani magwiridwe a 0,4-0.7 a Bisdisilfide (2,5-dimethyl-2,5-Bis (Tert-Butylperoxy) Hexane).
Makasitomala ayenera kusankha kutentha koyenera komanso nthawi yochiritsa kukula kwa kukula kwa malonda ndi njira yochiritsa.
Paketi Yogulitsa:
Izi sizowopsa, zimakhala m'malo mwa kadi kaditoni, pulasitiki, ma kilogalamu 10 pa thumba, matumba awiri pabokosi.
Zaka zosungirako:
Izi zimapangitsa kuti pakhale kuzizira, thumba liyenera kupewedwa kuti lisawonongeke poyendetsa kapena kugwiritsa ntchito.
Khalani m'malo ozizira, owuma ndi moyo wa alumali miyezi 12.