Fv9502
HERCHY
Availability: | |
---|---|
Quantitas: | |
PRAECIPUUS |
Index |
||
Vide |
Fv9552 |
Fv9562 |
|
Species Test modi |
luteolus |
||
Gravitas specifica / g / cm3 |
ASTM D792 |
1.42 |
1.43 |
Duritia / Shorea |
ASTM D2240 |
52 |
61 |
Tensile fortitudo / MPA |
Astm d412 |
10.2 |
9.4 |
Elongatio ad confractus /% |
Astm d412 |
330 |
280 |
Lacrimam viribus / kn / m |
ASTM D624-B |
20 |
19 |
Cogo Set (CLXXVII ℃ * 22h) |
Astm d395 |
7 |
8 |
Mollitiam /% |
Astm d1054 |
35 |
34 |
* Calor resistentia |
Duritio mutatio / litus a |
2 |
2 |
Duritio mutatio / litus a |
-24 |
-23 |
|
Elongatio ad confractus mutatio,% |
-21 |
-20 |
|
Fuel C |
ASTM D471 |
22 |
21 |
Curatio |
0,5 partes bis-2-5, unum gradu Vulcanisation CLXX ℃ × 15min, duo scaena Vulcanisation: CC ℃ × 4h |
Commendatur actiones:
Suus 'suggesserant utilitas 0.4-0.7 partes Bisdisulfide (2,5-Dimethyl, 2,5-bis (Tert, butylperoxy) Hexane).
Customers eligere maxime convenientem temperatus et tempus curationis fundatur in productum de magnitudine et modum curationis.
Product packaging:
Hoc productum est non periculo, suus 'pro composito ex Cardstock, plastic et X kilograms per peram, II sacculos per arca archa.
Age de repono:
Hoc productum habet a frigus flow capacitatem, sacculum vitandum ut non laedi per translationem vel utendo.
Ut in a frigus, arida environment cum fasciae vita XII mensibus.
PRAECIPUUS |
Index |
||
Vide |
Fv9552 |
Fv9562 |
|
Species Test modi |
luteolus |
||
Gravitas specifica / g / cm3 |
ASTM D792 |
1.42 |
1.43 |
Duritia / Shorea |
ASTM D2240 |
52 |
61 |
Tensile fortitudo / MPA |
Astm d412 |
10.2 |
9.4 |
Elongatio ad confractus /% |
Astm d412 |
330 |
280 |
Lacrimam viribus / kn / m |
ASTM D624-B |
20 |
19 |
Cogo Set (CLXXVII ℃ * 22h) |
Astm d395 |
7 |
8 |
Mollitiam /% |
Astm d1054 |
35 |
34 |
* Calor resistentia |
Duritio mutatio / litus a |
2 |
2 |
Duritio mutatio / litus a |
-24 |
-23 |
|
Elongatio ad confractus mutatio,% |
-21 |
-20 |
|
Fuel C |
ASTM D471 |
22 |
21 |
Curatio |
0,5 partes bis-2-5, unum gradu Vulcanisation CLXX ℃ × 15min, duo scaena Vulcanisation: CC ℃ × 4h |
Commendatur actiones:
Suus 'suggesserant utilitas 0.4-0.7 partes Bisdisulfide (2,5-Dimethyl, 2,5-bis (Tert, butylperoxy) Hexane).
Customers eligere maxime convenientem temperatus et tempus curationis fundatur in productum de magnitudine et modum curationis.
Product packaging:
Hoc productum est non periculo, suus 'pro composito ex Cardstock, plastic et X kilograms per peram, II sacculos per arca archa.
Age de repono:
Hoc productum habet a frigus flow capacitatem, sacculum vitandum ut non laedi per translationem vel utendo.
Ut in a frigus, arida environment cum fasciae vita XII mensibus.