FV9502 we de na di wɔl
Herchy bin de du am
| Di tin dɛn we yu kin gɛt: | |
|---|---|
| Kwantiti: . | |
Tin dɛn |
Index |
||
Serial nɔmba |
FV9552 we de na di wɔl |
FV9562 we de na di wɔl |
|
Aw a luk Di We dɛn fɔ Tɛst |
we gɛt yɔlɔsh |
||
Spesifi k Graviti/ g/cm3 |
ASTM D792 we yu de yuz |
1.42 |
1.43 |
Hadnɛs/shɔA |
ASTM D2240 we yu de yuz |
52 |
61 |
Tensile Strɔng/MPa |
ASTM D412 we yu kin yuz |
10.2 |
9.4 |
Elongation Na Brek /% . |
ASTM D412 we yu kin yuz |
330 |
280 |
Tiar Strɔng/KN/m |
ASTM D624-B we yu de yuz |
20 |
19 |
Set di kompreshɔn (177°C * 22h ). |
ASTM D395 we de na di wɔl |
7 |
8 |
Strɔng/% |
ASTM D1054 we gɛt fɔ du wit am |
35 |
34 |
*Hɛt rɛsistɛns |
Hadnes chenj /sho A |
2 |
2 |
Hadnes chenj /sho A |
-24 |
-23 |
|
Elongashɔn na brek chenj, % . |
-21 |
-20 |
|
Fiul C |
ASTM D471 we yu kin yuz |
22 |
21 |
Di Kɔndishɔn we de mɛn am |
0.5 pat dεm fכ bis-2-5, wan stej vulkanayzεshכn 170°C×15min, tu stej vulkanayzεshכn: 200°C×4h |
||
Di tin dɛn we dɛn kin du we dɛn kin du:
i sכgεst fכ yuz 0.4-0.7 pat dεm fכ bisdisulfayd (2,5-dimethyl-2,5-bis(tert-butylperoxy)hεksan).
Di kɔstɔma dɛn fɔ pik di tɛmpracha ɛn tɛm we fit pas ɔl fɔ mek dɛn mɛn am bay di sayz we di prɔdak gɛt ɛn di we aw dɛn fɔ mɛn am.
Di pak we dɛn de pak di prɔdak:
Dis prodak nɔ denja, insted na kadstɔk, plastic, ɛn 10 kilogram fɔ wan bag, 2 bag fɔ wan bɔks.
Di ej we dɛn dɔn kip am:
Dis prodak gɛt kol flɔ kapasiti, dɛn fɔ avɔyd di bag fɔ mek i nɔ pwɛl we dɛn de transpɔt ɔ yuz am.
Kip am na say we kol ɛn dray ɛn we go de fɔ 12 mɔnt.