FV9502
Herchy
Ho fumaneha: | |
---|---|
Bongata: | |
Lintho |
Index |
||
Nomoro ea letoto |
FV9552 |
FV9562 |
|
Ponahalo Mekhoa ea Teko |
o mosehla |
||
Gravity e itseng / g / cm3 |
Astm d792 |
1.42 |
1.43 |
Harness / Shorea |
Astm d2240 |
52 |
61 |
Matla a Tense / MPA |
Astm d412 |
10.2 |
9.4 |
Elong ea nako ea phomolo /% |
Astm d412 |
330 |
280 |
Matla a Toaar / Kn / m |
Astm d624-b |
20 |
19 |
Compression set (177 ℃ * 22h) |
Astm d395 |
7 |
8 |
Boithabiso /% |
Astm d1054 |
35 |
34 |
* Ho hanyetsa ho hanyetsa ho hanyetsa |
HarnessHent Change / Shore A |
2 |
2 |
HarnessHent Change / Shore A |
-24 |
-23 |
|
Ho nka nako ea ho khaola phetoho,% |
-21 |
-20 |
|
Fuel cor |
Astm d471 |
22 |
21 |
Boemo ba ho foqoha |
Likarolo tsa 0,5 tsa Bis-2-5, Mothati o mong oa Vis-20 ℃ × 15Mn, Mehato e 'Ngoe e Tšoara Mehato: 200 × |
Ketso tse khothalelitsoeng:
Ho khothalletsoa ho sebelisa likarolo tse 0,4-0.7 likarolo tsa bisdisulfide (2,5-disky, (Tort-butylperoxy) Hexane).
Bareki ba lokela ho khetha mocheso le nako e loketseng ho latela boholo ba sehlahisoa le mokhoa oa ho folisa.
Ho boloka lihlahisoa:
Sehlahisoa sena ha se kotsi, ho e-na le ho fuoa karete, polasetiki, le kilos tse 10 ka mokotla, mekotla e 2 ka lebokose.
Lilemo tsa polokelo:
Sehlahisoa sena se na le bokhoni bo batang bo batang, mokotla o lokela ho qojoa hore o se ke oa senyeha nakong ea lipalangoang kapa ts'ebeliso.
Boloka tikoloho e pholileng, e omileng e nang le bophelo ba sephali ba sephali ba likhoeli tse 12.
Lintho |
Index |
||
Nomoro ea letoto |
FV9552 |
FV9562 |
|
Ponahalo Mekhoa ea Teko |
o mosehla |
||
Gravity e itseng / g / cm3 |
Astm d792 |
1.42 |
1.43 |
Harness / Shorea |
Astm d2240 |
52 |
61 |
Matla a Tense / MPA |
Astm d412 |
10.2 |
9.4 |
Elong ea nako ea phomolo /% |
Astm d412 |
330 |
280 |
Matla a Toaar / Kn / m |
Astm d624-b |
20 |
19 |
Compression set (177 ℃ * 22h) |
Astm d395 |
7 |
8 |
Boithabiso /% |
Astm d1054 |
35 |
34 |
* Ho hanyetsa ho hanyetsa ho hanyetsa |
HarnessHent Change / Shore A |
2 |
2 |
HarnessHent Change / Shore A |
-24 |
-23 |
|
Ho nka nako ea ho khaola phetoho,% |
-21 |
-20 |
|
Fuel cor |
Astm d471 |
22 |
21 |
Boemo ba ho foqoha |
Likarolo tsa 0,5 tsa Bis-2-5, Mothati o mong oa Vis-20 ℃ × 15Mn, Mehato e 'Ngoe e Tšoara Mehato: 200 × |
Ketso tse khothalelitsoeng:
Ho khothalletsoa ho sebelisa likarolo tse 0,4-0.7 likarolo tsa bisdisulfide (2,5-disky, (Tort-butylperoxy) Hexane).
Bareki ba lokela ho khetha mocheso le nako e loketseng ho latela boholo ba sehlahisoa le mokhoa oa ho folisa.
Ho boloka lihlahisoa:
Sehlahisoa sena ha se kotsi, ho e-na le ho fuoa karete, polasetiki, le kilos tse 10 ka mokotla, mekotla e 2 ka lebokose.
Lilemo tsa polokelo:
Sehlahisoa sena se na le bokhoni bo batang bo batang, mokotla o lokela ho qojoa hore o se ke oa senyeha nakong ea lipalangoang kapa ts'ebeliso.
Boloka tikoloho e pholileng, e omileng e nang le bophelo ba sephali ba sephali ba likhoeli tse 12.