Fv9502 fluorosii -one

O lenei oloa e talafeagai mo le tui poʻo le suia o gaioiga, ma tulaga faʻapitoa e mafai ona fusia i le uʻamea, ammitrid ma isi mea. E i ai le atoatoa o le suauʻu tetee ma fofo revents. E matua maualalo le faʻamasinoga, o le teteʻe atu i le maualuga ma le maualalo o le vevela ma le maualalo, ma lelei le malosi.
  • FV9502

  • Jechy

Avanoa:
Aofaiga:

Togafitiga faapitoa

Mea

Faasino

Numera seriolo

Fv9552

FV9562

Foliga mai

Auala Sueina o Tafooga

samasama

Tuʻuina atu faʻapitoa / g / cm3

ASTM D792

1.42

1.43

Faigata / shorea

ASTM D2240

52

61

Tensile Malosi / MPA

Astm D412

10.2

9.4

Elongition i le malologa /%

Astm D412

330

280

Safu malosi / laka / m

ASTTM D624-B

20

19

Puia i le (177 ℃ * 22H)

ASTM D395

7

8

Maʻia /%

ASTM D1054

35

34

* Vevela tetee
225 ℃ × 72h

Faigata suiga / matafaga a

2

2

Faigata suiga / matafaga a

-24

-23

Faamutaina i le malologa suiga,%

-21

-20

Fuel C
volume suia /%
23 ℃ / 72h

ASTM D471

22

21

Malosiaga

0.5 vaega o BOD-2-5, tasi le tulaga Volcanisetion 170 ℃ × 15mi, lua tulaga eseese: 200 ℃ × 4h

FAUTUAINA GALUEGA:


Ua fautuaina e faʻaaoga le 0.4-0.7 vaega o Bisdesulfill (2,5-Dithedyl-2,5-Ber-Borllperooxy).


Tagata faʻatau e tatau ona filifilia le sili ona lelei le vevela ma le taimi mo le faʻafetaui i luga o le tele o oloa ma metotia o le gaoa.


Oloa afifiina:


O lenei oloa e le leaga, e le o iai i totonu o le paoa, palasitika, ma 10 kilokalama i le ato, 2 ato i le pusa.


Ioe o le teuina:


O lenei oloa e i ai le malulu tele, le ato e tatau ona 'alofia ina ia aua neʻi faʻaleagaina i le taimi o felauaiga poʻo le faʻaaogaina.


Ia tumau i se siosiomaga malu ma mago ma se fata fata o le 12 masina.


Talu ai: 
Le isi: 

Vave fesoʻotaʻiga

Tatou oloa

Fesootai Faamatalaga

Faaopopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +869 15221953351
Pule Tau Fatuga     2023 Shanghai Jerchy Comber Co., Ltd. Nofoaga 'ai |   Faalauaiteleina Faiga Faavae Pisinisi | Lagolagoina e Taʻitaʻi.