FV9700 Fluorosililicone .

Xiendliwa lexi xi lulamerile eka extrusion molding ya bis-disulfide. Yina ku tiya swinene ka mafurha, ku tiya ka solvent, ku tiya ka acid na alkali.
  • FV9700

  • Herchy

Ku kumeka:
Nhlayo: .

Swikombiso swa xithekiniki



Nchumu

Swikombiso

Nomboro ya xirhendzevutani

NFS9760

NFS9770

Xivumbeko

Maendlelo ya Swikambelo

Vuandlalo lebyi vonakaka, lebyi rhetaka, .

Ku hava thyaka

Nkoka wo karhi/ g/cm3

ASTM D792

1.44

1.48

Ku tiya/ribuwaA

ASTM D2240 ya xirhendzevutani

60

70

Ku tiya ka ku tsana/MPa

ASTM D412

10.5

10.1

Ku Elongation Hi Nkarhi wo Pfumala /% .

ASTM D412

207

201

Matimba ya ku handzuka/KN/m

ASTM D624-B ya xirhendzevutani

18

17

Seti ya Ntshikelelo(177°C * 22h)

Ku hambana ka ku tiya/A

+4

+5

Mpimo wa ku cinca ka matimba ya ku tsana/% .

-27

-24

Mpimo wa ku cinca ka ku leha/% .

-26

-23

Mafurha ya C

Ku Cinca ka Vholumo/% .

23°C/72h

ASTM D471

21

20

IRM903
Mpimo wa vholumo ya ku cinca/%
150°C×72h

ASTM D471

4.5

4

Nitric acid/sulfuric acid/hydrochloric acid leyi pfanganisiweke na xitofu PH2 100°C×120h

Ku lwisana na acid
Mpimo wa ku cinca ka vholumo/% .

ASTM D471

0.3

0.3

3% wa xitofu xa sodium hydroxide 60°C×72h

Ku lwisana na alkali
Mpimo wa ku cinca ka vholumo/% .

ASTM D471

0.4

0.3

Xiyimo xo Horisa

0.8 wa swiphemu swa bisditetra, vulcanisation ya xiteji xin’we 120°C×15min, vulcanisation ya switeji swimbirhi: 200°C×4h

Swiendlo leswi ringanyetiweke:


Ku ringanyetiwa ku tirhisa 0.4-0.7 wa swiphemu swa bisdisulfide (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).


Vaxavi vafanele ku hlawula mahiselo lawa ya faneleke swinene na nkarhi wo horisa kuya hi vukulu bya xiendliwa xikan’we na ndlela yo horisa.


Ku pakiwa ka swikumiwa:


Xiendliwa lexi a xi na khombo, ematshan’wini ya sweswo xi vumbiwa hi khadi, pulasitiki, na 10 wa tikhilogiramu hi nkwama, 2 wa minkwama hi bokisi.


Malembe ya vuhlayiselo: .


Xiendliwa lexi xina vuswikoti byo khuluka hi xirhami, nkwama wufanele ku papalatiwa leswaku wunga onhaki loko wu fambisiwa kumbe kutirhisiwa.


Hlayisa eka ndzhawu yo kufumela, yo oma leyingana vutomi bya 12 wa tinhweti.


Endzhaku: 
Landzelaka: 

XITLHOKOVETSELO XA XITLHANYI

SWILO SWA HINA

VUXOKOXOKO BYA VUXOKOXOKO

Engetelani: No.33, Lane 159, Gondzo ra Taiye, Xifundzha xa Fengxian, Shanghai
Riqingho / WhatsApp / Skype: +86 15221953351
Vukorhokeri bya Vutshila     2023 Shanghai Herchy Rubber Co., Ltd. Mepe wa sayiti |   Pholisi ya Vuhlayiseki | Nseketelo Hi Leadong.