GA-60X1A
Herchy
| samuwa: | |
|---|---|
| Yawan: | |
GA-60X1A Silicone Rubber mai jurewa zafi (250 da 300 OC) (HCR)
Aikace-aikace: dace da samar da auto sassa, zafi jure gadaje, zafi-resistant seals da sauran kayayyakin.
Maɓalli masu mahimmanci: kyakkyawan juriya na zafi da ƙarfin injina, ƙaddamar da amincin RoHS, REACH, da FDA.
Gwaji: 1% na wakili mai warkarwa (manna 50% na DBPMH a cikin danko silicone), 175°C x 5min x 15MPa.
| 250 digiri sigogi na samfur | |||||
| Samfura | GA-6041A | GA-6051A | GA-6061A | GA-6071A | |
| Bayyanar | Translucent | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Hardness (ShoreA) | 40 | 50 | 60 | 70 | |
| Girma (g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Ƙarfin ɗaure (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Tsawaita(%) | 700 | 600 | 500 | 400 | |
| Ƙarfin hawaye (kN/m) | 15 | 20 | 25 | 25 | |
| iska tsufa 250 ℃ x70H | Tauri | 45 | 54 | 64 | 75 |
| Ƙarfin tashin hankali | 6.2 | 7.3 | 7.5 | 6.5 | |
| Tsawaitawa | 380.0 | 300.0 | 280.0 | 200.0 | |