Mogala: +86 15221953351 Imeile: info@herchyrubber.com
Please Choose Your Language
DIHLAHISWA
O mo: Gae » Ditšweletšwa » Tlhamo ya Rabara » Silicone ya VMQ » GA-60X1A Rabara ya Silicone yeo e sa tsenego phišo (250 Le 300 OC) (HCR)

go rwala

Abelana go:
konopo ya go abelana ka facebook
konopo ya go abelana ka twitter
konopo ya go abelana ka mola
konopo ya go abelana ya wechat
linkedin arolelana konopo
konopo ya go abelana ka pinterest
konopo ya go abelana ka whatsapp
sharethis konopo ya go abelana

GA-60X1A Rabara ya Silicone yeo e sa kgonego go fiša (250 Le 300 OC) (HCR)

GA-60X1A Rabara ya Silicone yeo e sa kgonego go fiša (250 Le 300 OC) (HCR)
Kopo: e loketseng bakeng sa ho hlahisa likarolo koloi, mocheso-mahanyetsa cots, mocheso-resistantseals le dihlahiswa tse ling.
Dikarolo senotlolo: molemo mocheso resistanceand matla a mochine, feta theauthentication ya RoHS, REACH, le FDA.
  • GA-60X1A ya go dira bjalo

  • Herchy ya go swana le

Go hwetšagala:
Palo: .

GA-60X1A Rabara ya Silicone yeo e sa kgonego go fiša (250 Le 300 OC) (HCR)


Kopo: e loketseng bakeng sa ho hlahisa likarolo koloi, mocheso-mahanyetsa cots, mocheso-resistantseals le dihlahiswa tse ling.
Dikarolo senotlolo: molemo mocheso resistanceand matla a mochine, feta theauthentication ya RoHS, REACH, le FDA.
Teko: 1% ya moemedi wa go fodiša (50% ya peista ya DBPMH ka gare ga mare a silicone),175°C x 5min x 15MPa。


250 tekanyo Product ditekanyetos
Setšweletšwa GA - 6 0 4 1A GA - 6 0 5 1A GA - 6 0 6 1 A GA - 6 0 7 1A
Ponagalo E translucent
Williamplasticity ya go dira dilo 150 200 240 240
Thata (LebopoA) . 40 50 60 70
Kitlano (g / cm3) . 1.14 1.16 1.18 1.2
Matla a go goga (MPa) . 8.5 9 9.5 9
Go telefatšwa(%) . 700 600 500 400
Matla a go gagola (kN/m) . 15 20 25 25
moya botsofali 250 ° C x70H Thatafala 45 54 64 75
Matla a kgatelelo 6.2 7.3 7.5 6.5
Go telefatša 380.0 300.0 280.0 200.0


Peleng: 
Latelago: 

DIKGOKAGANO TŠA KA PELE

DIHLAHISWA TSA RONA

TSHEDIMOŠO YA KGOKAGANO

Add: No.33, Lane 159, Tsela ya Taiye, Setereke sa Fengxian, Shanghai
Mogala / WhatsApp / Skype: +86 15221953351 Mogala wa Sepedi
Tokelo ya ngwalollo e ileditšwe     2023 Shanghai Herchy Rabara Co., Ltd. Mmapa wa Sebaka |   Pholisi ya Sephiri | Thekgo Ka Leadong ya go iša.