GA-60X1A Mpira wa Silicone wosamva kutentha (250 Ndi 300 OC) (HCR)

GA-60X1A Mpira wa Silicone wosamva kutentha (250 Ndi 300 OC) (HCR)
Kugwiritsa ntchito: koyenera kupanga zida zamagalimoto, machira osagwira kutentha, zoletsa kutentha ndi zinthu zina.
Zofunika kwambiri: kukana kutentha kwabwino komanso mphamvu zamakina, kupititsa kutsimikizika kwa RoHS, REACH, ndi FDA.
  • GA-60X1A

  • Herchy

kupezeka:
kuchuluka:

GA-60X1A Mpira wa Silicone wosamva kutentha (250 Ndi 300 OC) (HCR)


Kugwiritsa ntchito: koyenera kupanga zida zamagalimoto, machira osagwira kutentha, zoletsa kutentha ndi zinthu zina.
Zofunika kwambiri: kukana kutentha kwabwino komanso mphamvu zamakina, kupititsa kutsimikizika kwa RoHS, REACH, ndi FDA.
Kuyesa: 1% ya machiritso (50% phala la DBPMH mu chingamu cha silicone), 175 ° C x 5min x 15MPa.


250 digiri Zogulitsa magawo
Zogulitsa Mtengo wa GA-6041A Mtengo wa GA-6051A Mtengo wa GA-6061A Mtengo wa GA-6071A
Maonekedwe Zowoneka bwino
Williamplasticity 150 200 240 240
Kuuma (ShoreA) 40 50 60 70
Kachulukidwe (g/cm3) 1.14 1.16 1.18 1.2
Mphamvu yamagetsi (MPa) 8.5 9 9.5 9
Kutalikira (%) 700 600 500 400
Mphamvu yamisozi (kN/m) 15 20 25 25
mpweya kukalamba 250 ℃ x70H Kuuma 45 54 64 75
Mphamvu yamphamvu 6.2 7.3 7.5 6.5
Elongation 380.0 300.0 280.0 200.0


Zam'mbuyo: 
Ena: 

MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.