Tijaabada: 1% ee wakiilka daawaynta (50% koollada DBPMH ee xanjada silikoonka),175°C x 5min x 15MPa.
| 250 darajo Alaabta | |||||
| Alaabta | GA-6041A | GA-6051A | GA-6061A | GA-6071A | |
| Muuqashada | Translucent | ||||
| Williamplasticity | 150 | 200 | 240 | 240 | |
| Adag ( ShoreA) | 40 | 50 | 60 | 70 | |
| Cufnaanta (g/cm3) | 1.14 | 1.16 | 1.18 | 1.2 | |
| Xoog xajin (MPa) | 8.5 | 9 | 9.5 | 9 | |
| Dheeraynta(%) | 700 | 600 | 500 | 400 | |
| Xoogga jeexjeexa (kN/m) | 15 | 20 | 25 | 25 | |
| hawada gabowga 250 ℃ x70H | Adag | 45 | 54 | 64 | 75 |
| Xoogga kacsanaanta | 6.2 | 7.3 | 7.5 | 6.5 | |
| Dheeraynta | 380.0 | 300.0 | 280.0 | 200.0 | |