GA-60X1A Kub-resistant Silicone Roj Hmab (250 Thiab 300 OC) (HCR)

GA-60X1A Kub-resistant Silicone Roj Hmab (250 Thiab 300 OC) (HCR)
Daim ntawv thov: tsim nyog rau kev tsim cov khoom pib, cov cots thaum tshav kub kub-resistant, kub-resistant seals thiab lwm yam khoom.
Cov yam ntxwv tseem ceeb: zoo tiv thaiv tshav kub thiab lub zog txhua yam, dhau qhov kev lees paub ntawm RoHS, REACH, thiab FDA.
  • GA-60X1A

  • Herchy

Muaj:
Quantity:

GA-60X1A Kub-resistant Silicone Roj Hmab (250 Thiab 300 OC) (HCR)


Daim ntawv thov: tsim nyog rau kev tsim cov khoom pib, cov cots thaum tshav kub kub-resistant, kub-resistant seals thiab lwm yam khoom.
Cov yam ntxwv tseem ceeb: zoo tiv thaiv tshav kub thiab lub zog txhua yam, dhau qhov kev lees paub ntawm RoHS, REACH, thiab FDA.
Kev kuaj: 1% ntawm tus neeg ua haujlwm kho (50% muab tshuaj txhuam ntawm DBPMH hauv cov pos hniav silicone), 175 ° C x 5min x 15MPa.


250 degree Product Parameters
Khoom Qauv TSIS MUAJ: GA-6041A Qauv TSIS MUAJ: GA-6051A Qauv TSIS MUAJ: GA-6061A Qauv TSIS MUAJ: GA-6071A
Qhov tshwm sim Translucent
Williamplasticity 150 200 240 240
Hardness (ShoreA) 40 50 60 70
Qhov ceev (g / cm3) 1.14 1.16 1.18 1.2
Tensile zog (MPa) 8.5 9 9.5 9
Elongation (%) 700 600 500 400
Lub zog tawg (kN / m) 15 20 25 25
huab cua laus 250 ℃ x70H Hardness 45 54 64 75
Lub zog tensile 6.2 7.3 7.5 6.5
Elongation 380.0 300.0 280.0 200.0


Yav dhau los: 
Tom ntej: 

QUICK LINKS

Peb cov khoom

Tiv tauj xov xwm