GA-60X1A Rubber Silicone pale wela (250 A me 300 OC) (HCR)

GA-60X1A Rubber Silicone pale wela (250 A me 300 OC) (HCR)
Hoʻohana: kūpono no ka hana ʻana i nā ʻāpana kaʻa, nā moena pale wela, nā mea pale wela a me nā huahana ʻē aʻe.
ʻO nā hiʻohiʻona nui: maikaʻi ka wela wela a me ka ikaika mechanical, hele i ka hōʻoia o RoHS, REACH, a me FDA.
  • GA-60X1A

  • Herchy

Loaʻa:
Nui:

GA-60X1A Rubber Silicone pale wela (250 A me 300 OC) (HCR)


Hoʻohana: kūpono no ka hana ʻana i nā ʻāpana kaʻa, nā moena pale wela, nā mea pale wela a me nā huahana ʻē aʻe.
ʻO nā hiʻohiʻona nui: maikaʻi ka wela wela a me ka ikaika mechanical, hele i ka hōʻoia o RoHS, REACH, a me FDA.
Ka ho'āʻo: 1% o ka lāʻau lapaʻau (50% paʻi o DBPMH i ka silicone gum), 175 ° C x 5min x 15MPa.


250 degere Nā palena huahana
Huahana GA-6041A GA-6051A GA-6061A GA-6071A
Ka nana aku Alohilohi
Williamplasticity 150 200 240 240
Paʻakikī (ShoreA) 40 50 60 70
Māmā (g/cm3) 1.14 1.16 1.18 1.2
Ka ikaika uʻi (MPa) 8.5 9 9.5 9
Elongation(%) 700 600 500 400
Kaha waimaka (kN/m) 15 20 25 25
ea kahiko 250 ℃ x70H ʻoʻoleʻa 45 54 64 75
Ka ikaika hoʻopaʻapaʻa 6.2 7.3 7.5 6.5
ʻO ka lōʻihi 380.0 300.0 280.0 200.0


Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.